19

You can see where around corners and even some straight runs it is peeling up. I'm running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I've trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

you are viewing a single comment's thread
view the rest of the comments
[-] 20inmyhead@lemmy.ml 6 points 9 months ago

Increase the temp on your first couple layers by 5°. I’ve found that really helps with adhesion. If you’re still having difficulty with certain prints try using a brim.

[-] BingoBangoBongo@midwest.social 2 points 9 months ago

This was the brim printing. But increasing temp did seem to help!

this post was submitted on 12 Jan 2024
19 points (100.0% liked)

3D Printing

4351 readers
1 users here now

For everyhting 3D printing related.

Please be excellent to each other :)

Icon by Freepik, Banner photo by Thiago Medeiros Araujo

founded 4 years ago
MODERATORS