this post was submitted on 09 Feb 2026
21 points (100.0% liked)

3DPrinting

21751 readers
8 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

Continuation from this Post: https://lemmy.blahaj.zone/post/36954883

After many of you Suggested that Heat could be a Potential Solution to Regaining Sanded PETG Colour, I got myself a Heatgun Capable of 600c°.

While it did Improve the Colouring, Especially for Darker parts it wasn't Enough. To be a bit more Specific, Both Green and Yellow Parts Fully did regain the Colour Red Improved a Lot, but not quite Satisfactory And Black did make a Difference, but its not Nearly Close enough, being a Matte Dark Gray instead of... Black

I've noticed that the Black only did regain its true Colour once actively Melting and Warping which doesn't help... Otherwise its a Light/Dark Gray Matte Black.

So I think the Heatgun Method doesn't quite hold for Dark Parts. What other Methods of Regaining Colour are there?

I do still have MEK that I could Try. I also Heard that Clearcoat could Work and that there are 3D Printing Specific Brands, should I give that a Shot?

you are viewing a single comment's thread
view the rest of the comments
[–] morbidcactus@lemmy.ca 2 points 2 weeks ago

Just make sure you've got good gloves/respiration and ventilation if you go MEK, as far as I recall it's not nearly as aggressive with petg like acetone and abs so going to take some time. The solvent method is by far the one I use the most often, I wet a rag or paper towel and take my time. I recall vapour smoothing being a thing too but that's going to need setup and the like.